471.75—Pretreatment standards for new sources (PSNS).
Except as provided in 40 CFR 403.7, any new source subject to this subpart which introduces pollutants into a publicly owned treatment works must comply with 40 CFR part 403 and achieve the following pretreatment standards for new sources (PSNS). The mass of wastewater pollutants in uranium forming process wastewater introduced into a POTW shall not exceed the following values:
(a) Extrusion spent lubricants—Subpart G—PSNS.
There shall be no discharge of process wastewater pollutants.
(b) Extrusion tool contact cooling water.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium extruded |
Cadmium |
0.007 |
0.003 |
Chromium |
0.013 |
0.005 |
Copper |
0.044 |
0.021 |
Lead |
0.010 |
0.005 |
Nickel |
0.019 |
0.013 |
Fluoride |
2.05 |
0.908 |
Molybdenum |
0.173 |
0.077 |
(c) Heat treatment contact cooling water.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of extruded or forged uranium heat treated |
Cadmium |
0.006 |
0.003 |
Chromium |
0.012 |
0.005 |
Copper |
0.040 |
0.019 |
Lead |
0.009 |
0.004 |
Nickel |
0.017 |
0.012 |
Fluoride |
1.86 |
0.827 |
Molybdenum |
0.158 |
0.070 |
(d) Forging spent lubricants—Subpart G—PSNS.
There shall be no discharge of process wastewater pollutants.
(e) Surface treatment spent baths.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium surface treated |
Cadmium |
0.006 |
0.002 |
Chromium |
0.010 |
0.004 |
Copper |
0.035 |
0.017 |
Lead |
0.008 |
0.004 |
Nickel |
0.015 |
0.010 |
Fluoride |
1.62 |
0.718 |
Molybdenum |
0.137 |
0.061 |
(f) Surface treatment rinse.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium surface treated |
Cadmium |
0.068 |
0.027 |
Chromium |
0.125 |
0.051 |
Copper |
0.432 |
0.206 |
Lead |
0.095 |
0.044 |
Nickel |
0.186 |
0.125 |
Fluoride |
20.1 |
8.90 |
Molybdenum |
1.70 |
0.752 |
(g) Wet air pollution control scrubber blowdown.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium surface treated |
Cadmium |
0.0007 |
0.0003 |
Chromium |
0.001 |
0.0005 |
Copper |
0.005 |
0.002 |
Lead |
0.001 |
0.0005 |
Nickel |
0.002 |
0.001 |
Fluoride |
0.208 |
0.092 |
Molybdenum |
0.018 |
0.008 |
(h) Sawing or grinding spent emulsions.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium sawed or ground with emulsions |
Cadmium |
0.001 |
0.0005 |
Chromium |
0.002 |
0.0009 |
Copper |
0.007 |
0.004 |
Lead |
0.002 |
0.0008 |
Nickel |
0.003 |
0.002 |
Fluoride |
0.338 |
0.150 |
Molybdenum |
0.029 |
0.013 |
(i) Sawing or grinding contact cooling water.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium sawed or ground with contact cooling water |
Cadmium |
0.033 |
0.013 |
Chromium |
0.061 |
0.025 |
Copper |
0.211 |
0.101 |
Lead |
0.046 |
0.022 |
Nickel |
0.091 |
0.061 |
Fluoride |
9.82 |
4.36 |
Molybdenum |
0.830 |
0.368 |
(j) Sawing or grinding rinse.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of sawed or ground uranium rinsed |
Cadmium |
0.001 |
0.0004 |
Chromium |
0.002 |
0.0007 |
Copper |
0.006 |
0.003 |
Lead |
0.002 |
0.0006 |
Nickel |
0.003 |
0.002 |
Fluoride |
0.277 |
0.123 |
Molybdenum |
0.024 |
0.011 |
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium formed |
Cadmium |
0.009 |
0.004 |
Chromium |
0.016 |
0.007 |
Copper |
0.055 |
0.026 |
Lead |
0.012 |
0.006 |
Nickel |
0.024 |
0.016 |
Fluoride |
2.56 |
1.14 |
Molybdenum |
0.216 |
0.096 |
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium formed |
Cadmium |
0.009 |
0.004 |
Chromium |
0.017 |
0.007 |
Copper |
0.057 |
0.027 |
Lead |
0.013 |
0.006 |
Nickel |
0.025 |
0.017 |
Fluoride |
2.64 |
1.17 |
Molybdenum |
0.223 |
0.099 |
Subpart G—PSNS
|
mg/employee—day |
Cadmium |
5.24 |
2.10 |
Chromium |
9.70 |
3.93 |
Copper |
33.6 |
16.0 |
Lead |
7.34 |
3.41 |
Nickel |
14.4 |
9.70 |
Fluoride |
1,560 |
692 |
Molybdenum |
132 |
58.4 |
(n) Degreasing spent solvents—Subpart G—PSNS.
There shall be no discharge of process wastewater pollutants.
Code of Federal Regulations
[50 FR 34270, Aug. 23, 1985; 51 FR 2888, Jan. 22, 1986]
Except as provided in 40 CFR 403.7, any new source subject to this subpart which introduces pollutants into a publicly owned treatment works must comply with 40 CFR part 403 and achieve the following pretreatment standards for new sources (PSNS). The mass of wastewater pollutants in uranium forming process wastewater introduced into a POTW shall not exceed the following values:
(a) Extrusion spent lubricants—subpart G—PSNS.
There shall be no discharge of process wastewater pollutants.
(b) Extrusion tool contact cooling water.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium extruded |
Cadmium |
0.007 |
0.003 |
Chromium |
0.013 |
0.005 |
Copper |
0.044 |
0.021 |
Lead |
0.010 |
0.005 |
Nickel |
0.019 |
0.013 |
Fluoride |
2.05 |
0.908 |
Molybdenum |
0.173 |
0.077 |
(c) Heat treatment contact cooling water.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of extruded or forged uranium heat treated |
Cadmium |
0.006 |
0.003 |
Chromium |
0.012 |
0.005 |
Copper |
0.040 |
0.019 |
Lead |
0.009 |
0.004 |
Nickel |
0.017 |
0.012 |
Fluoride |
1.86 |
0.827 |
Molybdenum |
0.158 |
0.070 |
(d) Forging spent lubricants—subpart G—PSNS.
There shall be no discharge of process wastewater pollutants.
(e) Surface treatment spent baths.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium surface treated |
Cadmium |
0.006 |
0.002 |
Chromium |
0.010 |
0.004 |
Copper |
0.035 |
0.017 |
Lead |
0.008 |
0.004 |
Nickel |
0.015 |
0.010 |
Fluoride |
1.62 |
0.718 |
Molybdenum |
0.137 |
0.061 |
(f) Surface treatment rinse.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium surface treated |
Cadmium |
0.068 |
0.027 |
Chromium |
0.125 |
0.051 |
Copper |
0.432 |
0.206 |
Lead |
0.095 |
0.044 |
Nickel |
0.186 |
0.125 |
Fluoride |
20.1 |
8.90 |
Molybdenum |
1.70 |
0.752 |
(g) Wet air pollution control scrubber blowdown.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium surface treated |
Cadmium |
0.0007 |
0.0003 |
Chromium |
0.001 |
0.0005 |
Copper |
0.005 |
0.002 |
Lead |
0.001 |
0.0005 |
Nickel |
0.002 |
0.001 |
Fluoride |
0.208 |
0.092 |
Molybdenum |
0.018 |
0.008 |
(h) Sawing or grinding spent emulsions.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium sawed or ground with emulsions |
Cadmium |
0.001 |
0.0005 |
Chromium |
0.002 |
0.0009 |
Copper |
0.007 |
0.004 |
Lead |
0.002 |
0.0008 |
Nickel |
0.003 |
0.002 |
Fluoride |
0.338 |
0.150 |
Molybdenum |
0.029 |
0.013 |
(i) Sawing or grinding contact cooling water.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium sawed or ground with contact cooling water |
Cadmium |
0.033 |
0.013 |
Chromium |
0.061 |
0.025 |
Copper |
0.211 |
0.101 |
Lead |
0.046 |
0.022 |
Nickel |
0.091 |
0.061 |
Fluoride |
9.82 |
4.36 |
Molybdenum |
0.830 |
0.368 |
(j) Sawing or grinding rinse.
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of sawed or ground uranium rinsed |
Cadmium |
0.001 |
0.0004 |
Chromium |
0.002 |
0.0007 |
Copper |
0.006 |
0.003 |
Lead |
0.002 |
0.0006 |
Nickel |
0.003 |
0.002 |
Fluoride |
0.277 |
0.123 |
Molybdenum |
0.024 |
0.011 |
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium formed |
Cadmium |
0.009 |
0.004 |
Chromium |
0.016 |
0.007 |
Copper |
0.055 |
0.026 |
Lead |
0.012 |
0.006 |
Nickel |
0.024 |
0.016 |
Fluoride |
2.56 |
1.14 |
Molybdenum |
0.216 |
0.096 |
Subpart G—PSNS
|
mg/off-kg (pounds per million off-pounds) of uranium formed |
Cadmium |
0.009 |
0.004 |
Chromium |
0.017 |
0.007 |
Copper |
0.057 |
0.027 |
Lead |
0.013 |
0.006 |
Nickel |
0.025 |
0.017 |
Fluoride |
2.64 |
1.17 |
Molybdenum |
0.223 |
0.099 |
Subpart G—PSNS
|
mg/employee—day |
Cadmium |
5.24 |
2.10 |
Chromium |
9.70 |
3.93 |
Copper |
33.6 |
16.0 |
Lead |
7.34 |
3.41 |
Nickel |
14.4 |
9.70 |
Fluoride |
1,560 |
692 |
Molybdenum |
132 |
58.4 |
(n) Degreasing spent solvents—subpart G—PSNS.
There shall be no discharge of process wastewater pollutants.
Code of Federal Regulations
[50 FR 34270, Aug. 23, 1985; 51 FR 2888, Jan. 22, 1986]